Product brief introduction
This steel has a low hardness during normalizing and a high processing roughness; however, it is heated at a relatively high temperature, and is normalized by means of a diffused air-cooling method after the furnace is baked to obtain a uniform fine-grained pearlite-ferrite structure. To achieve satisfactory machinability.
Product Parameter
C:0.47~0.55
Si:0.17~0.37
Mn:0.60~0.90
B:0.0005~0.0035
Technical Equipment
技术装备