Product brief introduction
2B11Aluminum alloy for rivet.
2 bl1 aluminum alloy with medium shear strength, heat treatment reinforcement, after annealing, quenching and hot plasticity is good, the rivet must be within 2 h after quenching riveting。
Product Parameter
铝 Al :余量
硅 Si :≤0.50
铜 Cu :3.8~4.5
镁 Mg:0.40~0.8
锌 Zn:≤0.10
锰 Mn:0.40~0.8
钛 Ti :≤0.15
铁 Fe: 0.000~0.500
注:单个:≤0.05;合计:≤0.10