Product brief introduction
The machinability of the steel is good, and the forging and heat treatment process performance is also good, and the grain growth, oxidization, decarburization and heat treatment deformation tendencies are smaller when heated.
Product Parameter
C:0.42~0.49
Si:0.17~0.37
Mn:1.10~1.40
B:0.0005~0.0035
P:≤0.035
S:≤0.035
Cu:≤0.030
Cr:≤0.030
Ni:≤0.30
Mo:≤0.15