Product brief introduction
The common quality defects of bearing parts after heat treatment include: quenched microstructures are overheated, underheated, quenched cracks, insufficient hardness, heat-treated deformation, surface decarburization, and soft spots.
Product Parameter
C: 0.37 to 0.44
Si: 0.17 to 0.37
Mn: 0.50 to 0.80
S: Permissible residual content ≤ 0.025
P : Permissible residual content ≤ 0.025
Cr: 0.60 to 0.90
Ni: 1.25 to 1.65
Cu: Permissible residual content ≤ 0.25
Mo: 0.15 to 0.25
Technical Equipment
技术装备